Sign In | Join Free | My himfr.com |
|
Ask Lasest Price | |
Brand Name : | ARCHTEX |
Model Number : | LC8258 |
Certification : | SGS |
Price : | Negotiable |
Payment Terms : | L/C, T/T, Western Union |
Supply Ability : | 1000 Metric Tons/Metric Ton per month |
Delivery Time : | 5-8 working days |
Composite heat calcium zinc stabilizer without sulfide contamination enviromental friendly
Product Features:
1. Environmental friendly products
No heavy metal elements (lead, septum), no toxic and hazardous
substances, can meet the requirements of the latest environmental
standards of various countries (such as the EU RHOS Directive,
REACH Directive, etc.).
2. No sulfur contamination
Products using lead salt stabilizers are prone to sulfur
contamination in the presence of sulfur (such as acid rain,
packaging boxes), causing yellowish discoloration or even
blackening of white products, seriously affecting the appearance.
Calcium and zinc stabilizers do not appear to behave like this
3. Good thermal stability
With the continuous development and improvement of calcium-zinc
stabilizers, it can basically replace the lead-salt composite
stabilizer with 1:1 to ensure the production cycle and stability.
After the cooling of the die, the material decomposition will
become quite slow.
4. Good system switching characteristics
Calcium-zinc heat stabilizers do not react with lead salts,
organotin and other heat stabilizers, will not cause pollution, and
have low switching costs, and will not affect the use of small
tubes, plastic steel and other recycled materials.
5. The product has no smell
PVC products produced by calcium-zinc stabilizers do not produce
odors with organotin, which is more acceptable to the public.
6. Low density, can increase the amount of calcium carbonate,
reduce costs.
The calcium-zinc heat stabilizer itself has a lower density than
the lead salt stabilizer, and the PVC product only has a decrease
in the weight of the heat stabilizer.
7. Promote foaming, reduce density
The raw material of calcium-zinc stabilizer, zinc stearate can
promote the decomposition of the foaming agent, make the foamed
product more delicate, and the density becomes smaller, and even
more, the dosage of the adjusting agent can be reduced, and the
cost is saved.
8. To prevent the generation of black lines
Although the organotin stabilizer has good thermal stability, it
does not have lubricity and plasticization is easy to produce black
wire (drag black). The calcium-zinc stabilizer has self-lubricating
properties and plasticization is adjustable, which can effectively
prevent The generation of black lines caused by problems such as
equipment and plasticization.
Technical Specifications:
Item | Index |
Character&appearance | white powder |
Metal oxide content%, ≥ | 20 |
Thermal stability time, ≥ | 80 |
Volatile%, ≤ | 1 |
Applications:
LC8258 is suitable for soft, semi-rigid non-toxic PVC products, especially for PVC pipe fitting
Recommended dosage:
raw material name | Reference amount |
PVC | 100 |
Caco3 | Appropriate amount |
Stabilizer | 4-6 |
other | Appropriate amount |
Packaging and storage:
25Kg paper bag, stored under room temperature and dry condition
Cautions:
1.This product is heat stabilizer for PVC processing, non flammable and explosive;
2.This product should be prevented from entering eyes, if splashing on skin should be washed with soap in time, the workplace should be well ventilated, directly inhalation of dust should be avoided during production and operation.
![]() |